Specification of drums of 83 cm in height with 150 kg net capacity:
Our factory uses the raw material with the best quality. Our factory uses steel sheets of Mobarakeh steel company in order to make steel drums. The important factors of our steel drums are plate thickness (body, top & bottom) 0.6+/- 0.02mm, Height 98 and 83 cm, Diameter 50 cm , Lid hole position, Lid hole diameter, Body corrugations, net filling capacity, gross weight, Drum tare weight and color.
158 kgs Drums for bitumen
Softening point of this grade is 42 to 52 or 45 to 52 0C base on ASTM D36.
Iran Bitumen
Feedar Esfahan Company is able to pack and export bitumen from best Iranian refineries such as The Arak refinery, The Esfahan refinery, The Qom refinery and The Shiraz refinery. The goal of Feedar Esfahan Company is Customer satisfaction by providing the best Iran bitumen in best possible packings along with the best prices. You can buy various high quality bitumen from Iran bitumen manufacturer, Feedar Esfahan. If you are looking for Iran bitumen price list daily or weekly, you can contact us by email of Feedar Esfahan company or contact form on this site and submit your request.
The specifications of penetration bitumen grades:
.
The specifications of penetration bitumen 60/70
.
The specifications of penetration bitumen 85/100
.
The specifications of penetration bitumen 40/50
.
The specifications of penetration bitumen 30/40
.
The specifications of penetration bitumen 80/100
.
The specifications of penetration bitumen 50/70
.
The specifications of penetration bitumen AH-70
.
The specifications of penetration bitumen AH-90
.
The specifications of Cutback Bitumen Grade MC-250
.
The specifications of Oxidized Bitumen Grade R85/25
.
The specifications of Oxidized Bitumen Grade R90/15
.
.
Visit English page(Iranian Bitumen Supplier) Iran Bitumen Marketing
技术信息渗透沥青:
在分析渗透沥青的所有等级的质量,即突出从其余的参数是石蜡含量。 在实验室测试中,石蜡趋于结晶在零摄氏度的温度。 在寒冷的气候条件下,这将导致在沥青颗粒变得非常脆导致它们拆散和路面损坏。 此外,在温度高于30℃,石蜡,作为油性的性质,导致在所得的沥青颗粒在彼此在高张力的滑动并产生的挥手路面特性沥青的粘合性的显着降低路的区域。
在当今世界上使用的原料价格高,因此只似乎是合乎逻辑使用能产生路面表面上的持续时间最长的沥青涂层的沥青,这是无法实现的,除非沥青的石蜡含量降低到2%以下。 在不断持续的斗争,以达到最好的质量,伊斯法罕炼油厂已经能够实现这一目标,我们很自豪地介绍渗透沥青所有等级与低于2%的石蜡含量。 石蜡这样的低电平将大大增加沥青颗粒的粘附和减少沥青的机会分手导致持久沥青涂层,其将,从长远来看,大大降低了道路维护成本的形成。
。
欲了解更多信息,请访问以下链接:
-
沥青60/70 | ||
测试方法 | 规范 |
|
D-70 | 1.01-1.06 | 比重@ 25/25℃ |
D-5 | 60/70 | 渗透@ 25℃ |
D-36 | 49/56 | 软化点C |
D-113 | 100分钟 | 延展性@ 25℃ |
D-6 | 最大0.2 | 加热(重量)%的损失 |
D-6&D-5- | 20最大 | 加热%,此前下降的渗透 |
D-92 | 250min | 闪点C |
D-4 | 99.5分钟 | 溶解度CS2(重量)% |
* AASHOT102 | 负 | 抽查 |
DIN-52015 | 小于2% | 石蜡含量 |